Altın Çıkartma altın kaplamalı söketlerden

Friends, the sockets didn't come out as I hoped. I was hoping for 5 or more, but you can't just hope for these things. Each socket can come out at a different rate. The acids I used in this process: 5 liters nitric acid 1 liter sulfuric acid 300 ml hydrochloric acid 30 ml hydrazine hydroxide I HAD PROCESSED THESE SOCKETS WITH ANY LIQUIDITY. I HAVE AN ESTIMATED 1000 TL REMAINING. I SENT THE 1400 TL TO THE FRIEND WHO SENT THE SOCKETS. MY INTEGRATED GOLD EXTRACTION VIDEO IS IN THE LINK BELOW    • Altın Çıkartma Entegrelerden nasıl altın ç...