Zinc Plating Take TWO | Roundtail Restoration

Yup, my fault. But, at least I see a light at the end of the tunnel. Lets get some hardware zinc plated. Here's what I used: Bench power supply (many available on Amazon) Aquarium Agitator: https://www.amazon.com/dp/B0BFHDTQFN?... Aquarium Heater: https://www.amazon.com/dp/B07H2MSRP8?... Zinc Plates: https://www.amazon.com/dp/B0CWRT64TS?... Epsom Salt: amazon.com/dp/B0BXTS6L35 pH Test Strips: https://www.amazon.com/dp/B0CW2H2HJY?... Zinc Sulfate Monohydrate: https://www.amazon.com/dp/B00T6I1SKS Various buckets, distilled water, wires, etc. Here's Steve's blog: https://www.nonlintec.com/tr4a/plating/ Caswell Surface Area Calculator: https://caswellplating.com/surface.ht... 00:00 - Intro 00:34 - Backstory 02:05 - Witch's Brew 05:16 - Mixing It Up 06:31 - Let There Be Heat 09:28 - Add the Battery Acid 10:14 - Zinc Plates 10:38 - My Mistake 12:28 - The First Bolt 13:07 - Removing Old Zinc 14:59 - Magic Bubbles 17:23 - Electrical Connections 21:39 - And We're Plating! 22:41 - 8 Minutes Later... 23:35 - Plating Done 23:46 - Focus!! 25:12 - Final Results 27:35 - Outro